EVALUATION OF ACID-GENERATING POTENTIAL OF COMPLEX MINE WASTES

LEVITAN, Denise M.1, SEAL, Robert R. II2, PIATAK, Nadine M.2, and HAMMARSTROM, Jane M.2, (1) US Geological Survey, 954 National Center, Reston, VA 20192, dlevitan@usgs.gov, (2) U.S. Geological Survey, 954 National Center, Reston, VA 20192

Acid-base accounting (ABA) is a static test commonly used in the prediction of acid production from mine wastes. In standard ABA, acid-generating potential (AP) is calculated from total sulfur content; modified ABA uses sulfide sulfur. It is assumed in the calculation of AP that the measured sulfur is derived from pyrite, yet this calculation can be inaccurate in mine wastes containing other sulfur-bearing minerals such as jarosite, pyrrhotite, gypsum, and sulfate salts. This study used a variety of leaching techniques on a representative suite of metal mine-waste samples (total S: 0.7 – 27 Wt. %) and mineral separates to understand the behavior of these minerals in order to determine accurate AP values. Six non-sequential leaches included water for soluble salts; both dilute and concentrated HCl targeting gypsum, jarosite, and pyrrhotite; Na2CO3 for gypsum and jarosite; NaOH for all sulfates; and HNO3 for pyrite. Qualitative and quantitative x-ray diffraction (XRD), sulfur measurements on solid residues, and sulfate measurements of leachates were used to assess the persistence of sulfur-bearing minerals following these leaches.

XRD showed removal of jarosite by boiled concentrated HCl, by Na2CO3, and by NaOH; of pyrrhotite by boiled concentrated HCl; and of gypsum by boiled concentrated HCl, by Na2CO3, and by HNO3. Incomplete removal of gypsum was seen following dilute HCl and NaOH treatments. In samples with high pyrite content, pyrite persisted throughout all the leaches, though a decrease in sulfur concentration was seen in samples treated with HNO3. It is possible, therefore, to distinguish the sulfides pyrite and pyrrhotite through a boiled concentrated HCl leach and to separate these sulfides from sulfates such as jarosite and gypsum through a Na2CO3 leach. Gypsum and jarosite may be differentiated through a HNO3 leach. These results suggest that current widely accepted ABA protocols may yield inaccurate results depending upon the mineralogy of mine wastes. Interpretation of ABA results can be improved through mineralogical studies of mine wastes and through modifications to leaching protocols.

2007 GSA Denver Annual Meeting (28–31 October 2007)
General Information for this Meeting
Session No. 145--Booth# 133
The Environmental Geology and Geochemistry of Mineral Deposits: Best Practices for Effective Prediction, Mitigation, Closure, and Remediation (Posters)
Colorado Convention Center: Exhibit Hall E/F
8:00 AM-12:00 PM, Tuesday, 30 October 2007

Geological Society of America Abstracts with Programs, Vol. 39, No. 6, p. 404

© Copyright 2007 The Geological Society of America (GSA), all rights reserved. Permission is hereby granted to the author(s) of this abstract to reproduce and distribute it freely, for noncommercial purposes. Permission is hereby granted to any individual scientist to download a single copy of this electronic file and reproduce up to 20 paper copies for noncommercial purposes advancing science and education, including classroom use, providing all reproductions include the complete content shown here, including the author information. All other forms of reproduction and/or transmittal are prohibited without written permission from GSA Copyright Permissions.